Title: | Voltametria de chumbo em cortiça |
Authors: | Sousa, João Carlos Araújo de Carvalho Caldeira da Ponte e |
Advisors: | Vaz, António Manuel Neto |
Issue Date: | 2012 |
Publisher: | Universidade de Évora |
Abstract: | É mostrado o teor médio conhecido de cinzas e metais em cortiça amadia, bem
como o desvio-padrão e o número de referências bibliográficas. Nomeadamente de:
Ca, K, Al, P, Na, Fe, Mg, Mn, Cu, Zn, Pb, Cr e Cd. De destacar (20ppm±20ppm; 5)
para Pb.
Foi criado um novo método quimiométrico para análise de dados, aplicado à
voltametria-de-redissolução-anódica-de-impulso-diferencial. O novo método produziu
uma incerteza expandida de ±0.3321ppm (ca. 1.42 %). A diferença entre os resultados
do novo e do anterior método foi de 0.01ppm (23.41 e 23.40ppm). O limite-dedetecção
mudou de aproximadamente 4.8 para 4ppm e o desvio-padrão-relativo
aproximadamente de 9 para 6%.
A voltametria-de-redissolução-anódica-de-impulso-diferencial permitiu obter,
para o chumbo, o resultado de 52.85ppm±41.63ppm (77.36%) ou
32.00ppm±12.16ppm (37.98%), estudadas duas amostras de cortiça. Foi feita a
optimização paramétrica e comparação com a espectrometria de absorção atómica; ### ABSTRACT:
It is shown the known average concentration of ashes and metals in
reproduction cork, as well as the standard-deviation and the number of bibliographic
references. Namely of: Ca, K, Al, P, Na, Fe, Mg, Mn, Cu, Zn, Pb, Cr and Cd. A remark
is made to (20ppm±20ppm; 5) for Pb.
A new chemometric method was created for data analysis, applied to
differential-pulse-anodic-stripping-voltammetry. The new method produced an
expanded uncertainty of ±0.3321ppm (ca. 1.42 %). The difference between the new
and old method results was 0.01ppm (23.41 and 23.40ppm). The limit-of-detection
changed from approximately 4.8 for 4ppm and the relative-standard-deviation
approximately from 9 to 6%.
The differential-pulse-anodic-stripping-voltammetry allowed to have, for lead,
the result of 52.85ppm±41.63ppm (77.36%) or 32.00ppm±12.16ppm (37.98%), after
the study of two cork samples. The parametric optimization was made and atomic
absorption spectrometry was used for comparison. |
URI: | http://hdl.handle.net/10174/11699 |
Type: | doctoralThesis |
Appears in Collections: | BIB - Formação Avançada - Teses de Doutoramento
|